Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FLEX NORYL™ Resin WCD895 - Asia - (PPE+TPE) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for FLEX NORYL™ Resin WCD895 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Flex Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
FLEX NORYL™ WCD895 resin is a flexible, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL 1581 VW-1 requirement and 80C end use temperature rating as defined by UL 1581. FLEX NORYL WCD895 resin is intended for evaluation wire and cable jacketing applications. It has a Shore A Hardness reading of 89 and exhibits superior thermal stability, very low water absorption, robust tensile strength, tensile elongation, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 17 g/10min ASTM D 1238
Temperature 250 °C -
Load 10 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Stress at break 18 MPa ISO 527
Strain at break 50 % ISO 527
ASTM Data
Tensile Strength at Break 18 MPa ASTM D 638
Elongation at Break 180 % ASTM D 638
Shore A Hardness 89 - ASTM D 2240
Thermal propertiesValueUnitTest Standard
ISO Data
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1030 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Screw speed 15 - 85 rpm -
Characteristics
Additives
Flame retarding agent
Special Characteristics
Flame retardant
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com